In this video you can see the progression of the salt spray by M2Lab test after almost 1.000 hours. The developments are as to be expected so far.
- After 168 hours you can see some early signs of aluminium corrosion around the stainless steal boltheads.
- After 336 hours there are some minor signs around the Geomet bolthead.
- After 504 hours we find further development of deposits around the stainless steal boltheads
- After 672 hours only moderate further developments of aluminium corrosion around the stainless steal boltheads seems to halt
- After 960 hours still almost no signs of aluminium corrosion around the duplex and Delta protect boltheads
Another 500 hours to go…